Superalloy Stud Bolts

Nimonic 80A UNS N07080 GH4180 Studs Bolts 2.4952 on Sale

Nimonic 80A UNS N07080 GH4180 Studs Bolts 2.4952 on Sale
Product Details

Nimonic 80A Studs
Nimonic 80A studs is a metal rod or bar with threads on both sides. It also known as double-headed screws or studs, used to connect two parts together. General for mining machinery, bridges, cars, motorcycles, boiler steel structure, hanging tower, large span steel structure and large buildings. 

We tend to use studs when the parts need to remove frequently, because the thread will be worn if install and remove often, then we need to change the studs.

Nimonic 80A is a nickel-based superalloy composed of Ni-Cr. In the high temperature with good strength and very excellent corrosion resistance and oxidation resistance. These advantages make the Nimonic 80A widely used in aerospace, aerospace, power stations and transportation and other high temperature hot forging parts.
Nimonic 80A Chemaical composition:

Alloy

%

Ni

Cr

Fe

Mn

Si

P

S

Al

Ti

C

Co

B

Zr

Cu

625

Min.

Balance

18






1.0

1.8






Max.


21

3.0

1.0

1.0

0.02

0.015

1.8

2.7

0.1

2.0

0.008

0.15

0.2

Nimonic 80A Physical properties:

Density

8.19 g/cm3

Melting range

1320-1365℃

Nimonic 80A minimum mechanical properties in the room temperature:

Status

Tensile strength
  Rm N/mm2

Yield strength RP0.2N/mm2

Elongation A5 %

Nimonic 80A

930

620

20

If our nimonic 80a uns n07080 gh4180 studs bolts 2.4952 on sale caters to your requirement, welcome to contact our professional manufacturers and suppliers. Highly qualified products, competitive price and good after-sale service can be assured.